发明名称 COATING MATERIAL FOR TREATING END FACE OF JOINT OF CAST IRON PIPE
摘要 PROBLEM TO BE SOLVED: To obtain a coating material which forms a coating film excellent in adhesion to cast iron and mortar by compounding an epoxy resin which is liquid at a normal temperature and has a specified number of epoxy groups and a specified epoxy equivalent with an amine-base curative, a diluent and a body pigment. SOLUTION: This coating material comprises an epoxy resin (e.g. a bisphenol epoxy resin) which is liquid at normal temperature and has an epoxy equivalent of 170-250 and, on average, at least 1.5 epoxy groups per molecule, an amine- base curative (e.g. a modified m-xylenediamine-type curative) preferably having an active hydrogen equivalent of 90-100, a diluent (e.g. a toluene resin as a nonreactive diluent resin) and a body pigment (e.g. barium sulfate). A cast iron pipe is coated after the end face of its joint is coated with this coating material. This coating material is quickly cured to quickly develop its strengths and gives a coating film having high strengths and adhering well to a cast iron pipe and a mortar lining, thus giving excellent water-stopping properties to the end face of the pipe.
申请公布号 JP2000273391(A) 申请公布日期 2000.10.03
申请号 JP19990083463 申请日期 1999.03.26
申请人 KURIMOTO LTD;DAINIPPON TORYO CO LTD 发明人 AOKI NOBUO;SAITO MASAHIKO;MICHIURA YOSHISADA;TAME SHINICHIRO;YAMADA YOSHIO
分类号 F16L9/02;B05D7/14;B05D7/24;B28B21/94;C09D5/08;C09D163/00;F16L58/06;F16L58/10;(IPC1-7):C09D163/00 主分类号 F16L9/02
代理机构 代理人
主权项
地址