摘要 |
<p>PROBLEM TO BE SOLVED: To obtain a producing method of a laminated ceramic electronic component with has few defects and is superior in lifetime characteristics. SOLUTION: Ceramic materials are formed in to a sheet, and inner electrode materials are printed on the sheet. By laminating and sintering a plural of sheets, a ceramic element assembly 12 and inner electrodes 14 are formed. Outer electrodes 16, 18 are formed so that they can be connected at right angles to inner electrodes 14 in the planes which are arranged facing each other in the ceramic element assembly 12. As a result, this laminated ceramic electronic component 10 is manufactured. Before sintering the assembly, carbon is added at least to either of the ceramic material or the inner electrode material.</p> |