摘要 |
PCT No. PCT/JP96/02676 Sec. 371 Date Mar. 17, 1998 Sec. 102(e) Date Mar. 17, 1998 PCT Filed Sep. 18, 1996 PCT Pub. No. WO97/10920 PCT Pub. Date Mar. 27, 1997A circular blank made of a steel plate is lapped onto an Al-based plate in lapped areas of the Al alloy plate and another steel plate. Then, the three members are pressed by a pair of electrodes, and a welding current is allowed to flow between both the electrodes, thereby sequentially performing the melting of a current-supplied portion of the Al alloy plate and a portion near the current-supplied portion, the elimination of a molten portion by a partial bulgy deformation of the blank toward the Al alloy plate, the abutment of the bulgy deformed portion against the steel plate, and the resistance-welding between the bulgy deformed portion and the steel plate.
|