摘要 |
<p>PROBLEM TO BE SOLVED: To obtain a laminated structural body with excellent solvent barrier properties, solvent resistance and impact resistance and a container for a volatile compd. using the laminated structural body. SOLUTION: A resin compsn. layer (A) wherein 5-100 pts.wt. polyolefin resin (A2) are incorporated to 100 pts.wt. saponified product (A1) of an ethylene-vinyl acetate copolymer with an ethylene content of 10-70 mole % and a degree of saponification of at least 85 mole %, and a resin compsn. layer (B) wherein 0.5-40 pts.wt. saponified product (B2) of an ethylene-vinyl acetate copolymer with an ethylene content of 10-70 mole % and a degree of saponification of at least 85 mole % are dispersed to 100 pts.wt. polyolefin resin (B1), are laminated.</p> |