摘要 |
PCT No. PCT/JP92/01671 Sec. 371 Date Aug. 18, 1993 Sec. 102(e) Date Aug. 18, 1993 PCT Filed Dec. 21, 1992 PCT Pub. No. WO93/13152 PCT Pub. Date Jul. 8, 1993.A method for producing a high molecular weight aliphatic polyester, wherein: (A) 100 parts by weight of polyester (a) with a number average molecular weight of at least 10,000, and a weight average molecular weight of at least 30,000, and with end-groups that are substantially hydroxyl groups, and with a melting point of at least 60 DEG C., the polyester (a) having been obtained by reacting the following three ingredients: (i) a glycol ingredient; (ii) an aliphatic dicarboxylic acid ingredient; and (iii) a trifunctional or tetrafunctional ingredient reacts with (B) 0.1-3 parts by weight of a poly-isocyanate in a melted state of the polyester (a). The method provides a high molecular weight aliphatic polyester which has good properties and a melt viscosity required for molding and forming and has a wide molecular weight distribution. The high molecular weight aliphatic polyester is applicable to a variety of fields, such as films, moldings and formings, fibers, etc.
|
申请人 |
SHOWA HIGHPOLYMER CO., LTD. |
发明人 |
TAKIYAMA, EIICHIRO;HATANO, YOSHITAKA;FUJIMAKI, TAKASHI;SEKI, SHIGEKATU;HOKARI, TAKAO;HOSOGANE, TADAYUKI;HARIGAI, NORIAKI |