发明名称 METHOD FOR PRODUCING A SPHERICAL ION EXCHANGE RESIN
摘要 A method for producing a spherical crosslinked copolymer, which comprises polymerizing a monofunctional addition-polymerizable monomer and a polyfunctional addition-polymerizable monomer by suspension polymerization in an aqueous medium in the presence of a radical polymerization initiator of the following formula (a) or (b) which has a decomposition temperature for a half-life period of 10 hours within a range of from 60 to 120.degree.C and which is capable of forming at least four radical initiating points per molecule by the decomposition: (a) wherein R1 is a linear or branched C1-10 alkyl group, R2 is a n-substituted C4-15 hydrocarbon group, and n is an integer of at least 2, wherein the plurality of R1 per molecule may be the same or different; (R4-O-O?mR5 (b) wherein R4 is a linear or branched C1-10 alkyl group, R5 is a m-substituted C4-25 hydrocarbon group, and m is an integer of at least 2, wherein the plurality of R4 per molecule may be the same or different.
申请公布号 CA2111022(A1) 申请公布日期 1994.06.11
申请号 CA19932111022 申请日期 1993.12.09
申请人 MITSUBISHI KASEI CORPORATION 发明人 ITO, TSUYOSHI;WATANABE, JUNYA;SUGAWARA, TOYOKAZU
分类号 B01J39/20;C08F4/38;C08F8/00;C08F212/04;(IPC1-7):B01J39/20;B01J41/14;C08F2/18;C08F4/36 主分类号 B01J39/20
代理机构 代理人
主权项
地址