摘要 |
Aluminum nitride powder (28), possibly powdered glass (29) and aluminum oxide powder (23) are introduced into the molding cavity of a pressure matrix (26) for fabrication of a carrier body from aluminum nitride, whose surface is at least partially covered with aluminum oxide. Subsequently a pressure stamp (22) of the pressure tool (20) is introduced into the molded cavity of the pressure matrix (26). The powdered layers (28, 29, 30) are compressed and subsequently sintered, for instance for two hours at 1600 degrees C. in a neutral atmosphere. |