发明名称 |
Galling resistant austenitic stainless steel alloy |
摘要 |
A galling and corrosion resistant austenitic stainless steel alloy is disclosed containing in weight percent about - w/o - Carbon 0.25 Max. - Manganese 2.0-7.0 - Silicon 1.0-5.0 - Phosphorus 0.05 Max. - Sulfur 0.3 Max. - Chromium 12-20 - Nickel 2.0-7.75 - Molybdenum 3 Max. - Copper 3 Max. - Nitrogen 0.35 Max. - the balance being essentially iron. To attain its unique properties the alloy must be balanced so as to contain no more than about 10% ferrite. The % Ni+1/2(% Mn) must not be less than 5.5% and not greater than 1/8[11(% Si)+42], and the sum of the (% C+% N) is at least 0.15%. Care must be taken that when the amount of silicon present is less than about 2.25%, at least about 4.0% manganese is present.
|
申请公布号 |
US4814140(A) |
申请公布日期 |
1989.03.21 |
申请号 |
US19870062899 |
申请日期 |
1987.06.16 |
申请人 |
CARPENTER TECHNOLOGY CORPORATION |
发明人 |
MAGEE, JR., JOHN H. |
分类号 |
C22C38/58;(IPC1-7):C22C38/40 |
主分类号 |
C22C38/58 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|