发明名称 HYDROGENATION CATALYST FOR COAL TAR
摘要 A catalyst used for hydrogen treatment of coal tar is characterized in that about 10 to 30 weight percent of Mo oxides as first catalyst component and about 1 to 6 weight percent of Ni and/or Co as second catalyst component, both related to the total catalyst weight, are supported on a porous inorganic substrate consisting essentially of alumina or silica alumina, and in that the mean pore size is about 8 to 18 nm, the pore size distribution is such that …<IMAGE>… and the total pore surface is higher than about 100 m<2>/g. The invention includes a method of hydrogen treatment with use of the catalyst, and a method of producing a super needle coke suitable for the preparation of the graphite electrode, which consists in subjecting the hydrogenated oil resulting from such hydrogen treatment to delayed coking.
申请公布号 AU4738085(A) 申请公布日期 1986.03.20
申请号 AU19850047380 申请日期 1985.09.11
申请人 NIPPON KOKAN K.K. 发明人 TADASHI MURAKAMI;MIKIO NAKANIWA;YOSHIO NAKAYAMA;MITSUAKI MASUO
分类号 B01J23/88;B01J35/10;C10B55/00 主分类号 B01J23/88
代理机构 代理人
主权项
地址