The high temperature aging of polyamides is substantially improved by incorporating therein an antioxidant and an oxide of a metal of Group II or III of the Periodic Table, preferably a crystalline aluminosilicate such as a synthetic zeolite. The amount of antioxidant is preferably 1 to 5% and the amount of metal oxide is preferably 0.5 to 5%. Polyamides which can be stabilized in this way include Nylon-6, Nylon-11 and Nylon-12.
|