发明名称 SHAPE MEMORY COPPER ALLOY
摘要 PURPOSE:To make the resulting titled alloy inexpensive and easy to cut and to enable the melting and heat treatment in the air by providing a specified composition consisting of Mn, Zn and Cu. CONSTITUTION:This shape memory Cu alloy consists of, by weight, <=12% Mn, 26-44% Zn and 62-65% Cu. Al may be added to the alloy so as to provide a composition consisting of <=12% Mn, <=3% (X%) Al, (26-4X)-44% Zn and (62+3X)-(56-X)% Cu. The working (transformation) temp. of the ternary alloy is usually about -150 deg.C- room temp. The working temp. can be raised up to a temp. above room temp. by adding Al.
申请公布号 JPS5970742(A) 申请公布日期 1984.04.21
申请号 JP19820179657 申请日期 1982.10.12
申请人 OOSAKAFU 发明人 HANATACHI YUUKOU;MIYAGI MASAKAZU
分类号 C22C9/00;C22C9/04 主分类号 C22C9/00
代理机构 代理人
主权项
地址