摘要 |
<p>The paper is obtained by coating a biaxially drawn polypropylene film with a thickness of between 10 and 30 microns and an opacity of between 50 and 80%, the film having been made capable of attaching to a coat in an aqueous medium, the said coating being carried out by depositing from 4 to 10 g/m<2> and per face of a coat containing an opacifying filler, a printability filler, at least one latex binder and at least one heat-curable resin employed in a proportion of 5 to 20% by weight relative to the binder. The present invention also relates to the process for producing the said new paper.</p> |