发明名称 THIN AMORPHOUS MAGNETIC ALLOY PLATE FOR MAGNETIC HEAT AND CORE FOR MAGNETIC HEAD
摘要 PURPOSE:To obtain high saturation magnetic flux density, wear resistance and corrosion resistance in a thin amorphous magnetic alloy plate for a magnetic head, by adding prescribed amounts of Ru, Cr and Ti to Fe-Co-Ni alloy. CONSTITUTION:A thin amorphous magnetic alloy plate for a magnetic head is formed with a composition represented by the general formula, where M represents one or more of iron group elements, Ru, Cr and other transition metal elements except Ti, and X represents one or more of Si and other vitrifying element except B. Further, x+y+z+w+v+u=100at%, where y is 0.01-8at%, z 0.5-2at%, w 0.05-2at%, v 0-4at%, and u 20-26at%. In addition, p+q+r= 100%, k+1+m=100%, 100%, where p is 3-7%, r 0-10%, k 0.5-20%, and m 0-2%. The thin plate thus obtained has high saturation magnetic flux density, high wear resistance and high corrosion resistance.
申请公布号 JPS57198608(A) 申请公布日期 1982.12.06
申请号 JP19810084048 申请日期 1981.05.31
申请人 TOKYO DENKI KAGAKU KOGYO KK 发明人 OOYA KAZUO;ISHIJIMA NORIO
分类号 C22C45/04;G11B5/127;G11B5/147;G11B5/255;H01F1/153 主分类号 C22C45/04
代理机构 代理人
主权项
地址