发明名称 CONTINUOUS CASTING METHOD OF SHEET
摘要 PURPOSE:To make possible the large-volume production of the good-quality sheets of thicknesses about 3-20mm of much demand by making a pair of cooling rolls by copper and forming a pool by their top surfaces and a pair of side sealing members in the captioned method of pouring molten metal in the molten steel pool between a pair of cooling rolls. CONSTITUTION:The spacing between a pair of copper-made water-cooled rolls 1, 1 is adjusted according to the thickness of the slab to be produced and the molten steel 3 in a tundish 2 is poured up to the specified position of the molten metal level of the molten steel pool 4. Next, when the rolls 1, 1 are revolved in the specified (arrow) direction and in the specified velocity and pouring is continued, the molten steel in the pool 4 is quenched by making contact with the roll surfaces, thereby forming the solidified shells 6, 6 of chilled crystals. These are rolled by the rolls and become a slab 7 which is then continuously drawn. The pool 4 is formed by the top part surfaces mutually opposing along the roll axial direction and a pair of side part sealing members 5, 5 which are equipped by having a slight clearance from their top surfaces on the end parts on both sides of said top surfaces.
申请公布号 JPS55109549(A) 申请公布日期 1980.08.23
申请号 JP19790015050 申请日期 1979.02.14
申请人 MITSUBISHI HEAVY IND LTD 发明人 YOSHIHARA AKIYO;KADOI JIYUN;FUJIKAWA YASUO
分类号 B22D11/06 主分类号 B22D11/06
代理机构 代理人
主权项
地址