摘要 |
<P>PROCEDE POUR EXTRAIRE DES METAUX NON FERREUX DE MINERAI DE NICKEL LATERITIQUE PAR REDUCTION SELECTIVE DU MINERAI.</P><P>LES OPERATIONS DU PROCEDE SONT LES SUIVANTES:A.ON EFFECTUE UN BROYAGE 104 DU MINERAI DE NICKEL LATERITIQUE;B.ON FORME UN MELANGE DU MINERAI BROYE:1AVEC DU CHARBON BROYE A FORTE TENEUR EN SOUFRE ET EN SUBSTANCES VOLATILES 105-106;2AVEC UNE MATIERE SOUFREE NON GAZEUSE 107 QUI EST AJOUTEE EN QUANTITE TELLE QUE, EN TENANT COMPTE DU POIDS DE SOUFFRE CONTENU DANS LE CHARBON, LE POIDS TOTAL DE SOUFRE SOIT COMPRIS ENTRE 1 ET 1,5 DU POIDS DE MINERAI;C.ON CHARGE LE MELANGE DANS UNE CHAMBRE 109 DANS LAQUELLE L'AIR EST ESSENTIELLEMENT EXCLU;D.ON AUGMENTE LA TEMPERATURE (COMME EN 7) DU MELANGE DANS LA CHAMBRE JUSQU'A UNE VALEUR OU LA REDUCTION DES OXYDES DE METAUX NON FERREUX CONTENUS DANS LE MINERAI EST ESSENTIELLEMENT COMPLETE MAIS OU LES OXYDES DE FER DU MINERAI RESTENT ESSENTIELLEMENT INCOMPLETEMENT REDUITS.</P><P>APPLICATION AUX TRAITEMENTS DE MINERAIS.</P>
|