发明名称 MOLDING METHOD OF HOLLOW CONTAINERS
摘要 PURPOSE:To obtain a hollow container having improved dimensional stability and little shrinkage with time efficiently, by utilizing the instantareous temperature rise due to the adiabatic compression of air in molding the container from a thermoplastic resin according to the orientation blowing. CONSTITUTION:The preform 1 adjusted to the softening temperature is charged into the split molds 2 and 2 with the opening held, and air is blown into the preform 1 by advancing the piston 12 of the air cylinder 11 in the direction of arrow. When the piston 12 advances from the position A to the position B, the preform 1 is brought into contact with the cool surfaces 3 of the molds 2 and 2, molded into the form of the desired container, cooled, and solidified. When the piston 12 is advanced to the position C, the air in the container is pressurized, and the temperature rises rapidly, to heat the container to a temperature above the glass transition point, and the internal stress produced in the blow molding is removed. The release valve 6 is when opened to reduce the pressure, and the mold is opened to take out the container.
申请公布号 JPS54153867(A) 申请公布日期 1979.12.04
申请号 JP19780062158 申请日期 1978.05.26
申请人 DAINIPPON INK & CHEMICALS 发明人 TANIMOTO MASATSUGU
分类号 B29B11/08;B29B11/10;B29C49/04;B29C49/06;B29C49/08;B29C49/46;B29C49/64;B29C49/68;B29C49/78;B29C65/00;B29K67/00;B29L22/00 主分类号 B29B11/08
代理机构 代理人
主权项
地址