摘要 |
<p>Zinc and, if desired, lead are volatilized from a metallurgical material such as a finely divided oxidic ore, ore concentrate or another metallurgical intermediate. The volatilization of the zinc is carried out at a temperature above 1300 DEG C. in a cyclone chamber which has an axis that is substantially horizontal, i.e. is inclined to the horizontal at an angle of 0 DEG to 15 DEG . Carbon dioxide is removed from the gas leaving the zinc condensing stage and the high carbon monoxide gas thus obtained is recycled to the cyclone chamber or at another point ahead of the condensation stage.</p> |