摘要 |
To provide an alloy having high strength, toughness, and which is highly resistant to impact loading, the alloy has the following composition (all percentages by weight): 2-4.5 Mo, more than 2.5 to less than 3.5% Ni, more than 0.3 to less than 0.6% P, the rest iron; preferably, 3% Mo, 3% Ni, 0.45% P and the rest iron are used.
|