发明名称 Method for heat-treating steel rail head.
摘要 <p>A method for heat-treating a steel rail head, which comprises: heating a steel rail head to the austenization temperature; then, cooling the rail head by means of a hot water jet until a surface temperature of the rail head decreases to a temperature not below 420 DEG C; and then, cooling the rail head by means of an air jet at least to the pearlite transformation temperature, thereby transforming the structure of a surface portion of the rail head into a uniform and fine pearlite structure. The above-described method includes a method in which the rail head is previously cooled by means of a water spray until the surface temperature of the rail head decreases to a temperature not below 530 DEG C prior to the cooling of the rail head by means of the above-mentioned hot water jet.</p>
申请公布号 EP0293002(A1) 申请公布日期 1988.11.30
申请号 EP19880108529 申请日期 1988.05.27
申请人 NIPPON KOKAN KABUSHIKI KAISHA 发明人 TERAMOTO, TOYOKAZU NIPPON KOKAN K.K.;FUJIBAYASHI, AKIO NIPPON KOKAN K.K.;FUKUDA, KOZO NIPPON KOKAN K.K.;UEDA, MASAHIRO NIPPON KOKAN K.K.;NAGAHASHI, SHINICHI NIPPON KOKAN K.K.;KATAOKA, YUZURU NIPPON KOKAN K.K.;SATO, HIROAKI NIPPON KOKAN K.K.;WADA, TSUNEMI NIPPON KOKAN K.K.;GINO, TAKAO NIPPON KOKAN K.K.;SAITO, YOSHIO NIPPON KOKAN K.K.;MORIOKA, KIYOTAKA NIPPON KOKAN K.K.
分类号 C21D9/04;C21D1/19;(IPC1-7):C21D9/04 主分类号 C21D9/04
代理机构 代理人
主权项
地址