摘要 |
PROBLEM TO BE SOLVED: To provide a manufacturing method of flaky ferronickel capable of having a percentage of the flaky ferronickel having a maximum diameter of less than 20 mm of 90% or more in a ferronickel manufacturing.SOLUTION: A melting ferronickel is poured to a disc 11 having a diameter of 300 to 500 mm formed by a silicon carbide refractory containing alumina of 45 to 100% and alumina refractory or silicon carbide of 30 to 90%, the disc 11 is rotated at 150 to 300 rpm, and the melting ferronickel dispersed by the disc 11 is dropped into water and cooled. |