摘要 |
<p>The present invention provides spring-use heat treated steel which is cold coiled, can achieve both sufficient atmospheric strength and coiling workability, has a tensile strength of 2000 MPa or more, and can improve the performance as a spring by heat treatment after shaping the spring, that is, heat treated steel for high strength spring containing, by mass%, C: 0.45 to 0.9%, Si: 1.0 to 3.0%, Mn: 0.1 to 2.0%, V: over 0.1 to 1.0%, N: limited to 0.007% or less, and a balance of Fe and unavoidable impurities, and satisfying, in terms of the analyzed value of the extracted residue after heat treatment, [amount of V in filtrate filtered by 0.2 µm filter (mass%)]‰¥[amount of V in steel (mass%)]‰¥0.4.</p> |