摘要 |
<P>PROBLEM TO BE SOLVED: To provide a method for manufacturing an electrode mixture, by which an electrode mixture improved in ion conductivity can be manufactured. <P>SOLUTION: A method for manufacturing an electrode mixture containing an active material and an electrolyte includes, when a temperature at which the electrolyte is crystallized is denoted as T1, and a temperature at which the electrolyte begins to shrink under pressurization is denoted as T2, a first heat treatment step of heating a mixture including the active material and the electrolyte up to a temperature of T2 or above and less than T1 while pressurizing the mixture, and a second heat treatment step of heating the mixture up to a temperature of T1 or above after the first heat treatment step. <P>COPYRIGHT: (C)2013,JPO&INPIT |