发明名称 |
METHOD FOR PREPARING POLARIZER |
摘要 |
PURPOSE: A manufacturing method of a polarizer is provided to prevent degradation after putting under dry heat condition and to improve color durability. CONSTITUTION: A transparent non-oriented polyvinyl alcoholic film is precipitated in water of 30°C for 2 minutes, swelled and is dyed after being precipitated in a 30°C aqueous solution in which 3.5 mmol/L iodine and 2 weight% potassium iodide are included for dyeing for 4 minutes. The polyvinyl alcoholic film is precipitated in a 50°C cross-linking aqueous solution in which 10 weight% potassium iodide, 3.7 weight% boric acid and 0.5 weight% magnesium acetate are included for 2 minutes and is cross-linked. A cellulose triacetate is laminated on both surface of a polarizer and a polarizer plate is manufactured. |
申请公布号 |
KR20130030990(A) |
申请公布日期 |
2013.03.28 |
申请号 |
KR20110094628 |
申请日期 |
2011.09.20 |
申请人 |
DONGWOO FINE-CHEM CO., LTD. |
发明人 |
LEE, JONG SEOK;KIM, YUN SEONG;JO, CHEON HEE |
分类号 |
G02B5/30;G02F1/1335 |
主分类号 |
G02B5/30 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|