摘要 |
The present invention discloses a method for producing a positive electrode active material for a lithium secondary battery constituted by a lithium-nickel-cobalt-manganese complex oxide with a lamellar structure, the method including: (1) a step of preparing a starting source material for producing the complex oxide including a lithium supply source, a nickel supply source, a cobalt supply source, and a manganese supply source; (2) a step of pre-firing the starting source material by heating at a pre-firing temperature that has been set to a temperature lower than 800° C. and higher than a melting temperature of the lithium supply source; and (3) a step of firing the pre-fired material obtained in the pre-firing step by raising a temperature to a temperature range higher than the pre-firing temperature. |