发明名称 METHOD FOR PRODUCING POLYLACTIC ACID RESIN COMPOSITION
摘要 <P>PROBLEM TO BE SOLVED: To obtain favorable flexibility and heat resistance in a polylactic acid resin composition. <P>SOLUTION: In the method for producing the polylactic acid resin composition, a mixture containing the polylactic acid resin and surface-treated inorganic powder is kneaded by the use of the same direction-engaging biaxial extruder while conditions 1-3 are satisfied. The condition 1: a first temperature setting zone which is provided to include a range of at least 6.3D-13D mm from the central position of the raw material supply port of a barrel and in which the set temperature of the barrel is (Tm+50)-(Tm+80)&deg;C, and a conveyance element is provided in a screw; and a second temperature setting zone which is provided to include a range after at least 19.3D mm and in which the set temperature of the barrel is (Tm-20)-(Tm+40)&deg;C are provided. In the condition 2, in a range of 13D-20.9D mm, a first kneading part which has a length of 1D-4D mm and in which a kneading element is provided in the screw is provided. In the condition 3, in a range after 20.9D mm, a second kneading part which has a length of 1D-4D mm and in which a kneading element is provided in the screw is provided. <P>COPYRIGHT: (C)2012,JPO&INPIT
申请公布号 JP2012131072(A) 申请公布日期 2012.07.12
申请号 JP20100283537 申请日期 2010.12.20
申请人 KAO CORP 发明人 KISHIMOTO HIROAKI;TAKENAKA AKIRA
分类号 B29B7/90;B29B7/48;B29B7/72;C08J3/20;C08K9/00;C08L67/04;C08L101/16 主分类号 B29B7/90
代理机构 代理人
主权项
地址