发明名称 ENVIRONMENTAL LOAD-REDUCING MORTAR OR CONCRETE KNEADING MATTER
摘要 <p><P>PROBLEM TO BE SOLVED: To provide a cement-based material providing enormously high effect on reduction of CO<SB>2</SB>emission, and meeting strength applicable as the structural material of buildings, e.g.≥18 N/mm<SP>2</SP>of 28 days compression strength. <P>SOLUTION: This environmental load-reducing mortar or concrete kneading matter includes cement and an admixture as powdery components, has a water/powder ratio W/B of 20-46%, and a mass ratio (substitution rate) of the admixture occupied in the powder of 80-95%, and excels in suppression of residual unhydrated cement component after curing. One comprising one or more of blast furnace slag and fly ash can be used for the admixture. <P>COPYRIGHT: (C)2011,JPO&INPIT</p>
申请公布号 JP2010265166(A) 申请公布日期 2010.11.25
申请号 JP20100092190 申请日期 2010.04.13
申请人 KAJIMA CORP 发明人 SHINTANI AKIRA;KANDA TETSUSHI;OIZUMI KENJI;MOMOSE HARUMOTO;YODA KAZUHISA
分类号 C04B28/02;C04B18/08;C04B18/14 主分类号 C04B28/02
代理机构 代理人
主权项
地址