摘要 |
<p>A method is disclosed comprising in-mold coating a structural foam part made from a thermoplastic aromatic polycarbonate resin or a thermoplastic ABS polymer resin with a thermosetting in-mold coating composition at a pressure of from about 25 to 50 p.s.i. and at a temperature not in excess of about 200 DEG F. for from about 1 to 10 minutes, preferably for from about 1 to 3 minutes, to provide hard, smooth and adherent coatings, said thermosetting in-mold coating composition comprising an ethylenically unsaturated polyester resin and an ethylenically unsaturated monomer(s) catalyzed with an organic perioxide initiator including an accelerator for the initiator.</p> |