发明名称 MATERIAL FOR COMPOSITE MAGNETIC MEMBER, COMPOSITE MAGNETIC MEMBER USING THE MATERIAL, MANUFACTURING METHOD FOR THE MEMBER, AND MOTOR USING THE MEMBER
摘要 PROBLEM TO BE SOLVED: To form a weak magnetic part by carrying out heating treatment at a temperature lower than that in the case of a material for the conventional member, as a material for a composite magnetic member by which both magnetic properties of ferromagnetism and weak magnetism can be attained with a single composition. SOLUTION: The material is that for a composite magnetic member having a ferromagnetic part and a weak magnetic part with a single composition. The material has a composition consisting of, by mass,≤0.10% C, 0.10 to 2.0% Si, 0.10 to 4.0% Mn, >20.0% to <28.0% Ni and the balance essentially Fe and also has a martensitic structure, and further, the amount of spontaneous magnetization (J) under the external magnetic field of 1 T(tesla) is made to≥1.3 T. COPYRIGHT: (C)2004,JPO
申请公布号 JP2004091842(A) 申请公布日期 2004.03.25
申请号 JP20020253420 申请日期 2002.08.30
申请人 HITACHI METALS LTD 发明人 YOKOYAMA SHINICHIRO;SASAKI KAZU
分类号 C21D8/12;C22C38/00;C22C38/08;C22C38/58;H02K1/02;H02K19/10;(IPC1-7):C22C38/00 主分类号 C21D8/12
代理机构 代理人
主权项
地址