发明名称 STRAIGHTENING METHOD FOR ALPHA+BETA TYPE TITANIUM ALLOY STRAIGHT BAR
摘要 PROBLEM TO BE SOLVED: To straighten anα+βtype titanium alloy straight bar in relatively high productivity and to produce a straight bar having good straightness from a wire rod made of, particularly, anα+βtype titanium alloy. SOLUTION: By inserting a bar having bends straightened from a wire rod coil ofα+βtype titanium alloy in any container among a round shape, a circular arc shape, an U shape, an V shape in cross section and holding at a prescribed hold temp. of below theβtransformation temp. for a prescribed time or more, bends of the bar is not increased at heat treatment and is efficiently reduced, further, stabilized straightness is obtained after subsequent cold straightening, cutting and grinding of a surface.
申请公布号 JPH10291029(A) 申请公布日期 1998.11.04
申请号 JP19970101561 申请日期 1997.04.18
申请人 NIPPON STEEL CORP 发明人 TAKAHASHI KAZUHIRO;TAKAYAMA ISAMU;KAWAKAMI SATORU
分类号 B21D3/00;B21D3/12;B21F1/02;C22F1/00;C22F1/18;(IPC1-7):B21D3/00 主分类号 B21D3/00