摘要 |
PROBLEM TO BE SOLVED: To obtain a polycarbonate resin laminate simultaneously improved in weather resistance and coloring and transparency of a coating layer. SOLUTION: This laminate is constituted so that a thermoplastic resin, whose thickness is 10-150μm, coats the surface of a polycarbonate resin molding. In this case, the thermoplastic resin is a polycarbonate resin laminate including a specific ultraviolet rays absorbent formed of a hydroxyphenyltriazine based compound and satisfying the thickness of the coating layer thermoplastic resin layer(μm)×the concentration of ultraviolet rays absorbent in the coating layer(wt.%)=20-300. The coating layer thermoplastic resin is a polycarbonate resin or an acrylic resin. Then, the coating layer thermoplastic resin and the base material part polycarbonate resin have a mixed layer biting into each other between the coating layer thermoplastic resin of the laminate and the base material part polycarbonate resin molding. The thickness of the mixed layer is 0.1-2μm and the largest amplitude of a corrugation is 10μm or less per a 5mm of width.
|