The method coats a raw piece with an artificial pearl compound to be again coated with a ultraviolet paint to be irradiated with ultraviolet rays for increasing the surface hardening and the surface luster. The coating mixture comprises: cellulose acetate; acetone; amyl acetate, butyl acetate; pearl powder. The coated product is dried at 30-50 deg.C for 40-60 minutes.
|