发明名称 METHOD FOR CRUSHING WATER GRANULATED BLAST FURNACE SLAG
摘要 <p>PURPOSE:To increase the efficiency of crushing of water granulated blast furnace slag and the fineness of powder of the slag by using an auxiliary for crushing composed of limestone and diethylene glycol. CONSTITUTION:An auxiliary for crushing is added to water granulated blast furnace slag and this slag is crushed. The auxiliary is composed of 2-10wt.% limestone based on 100wt.% of the slag and 0.01-0.06wt.% diethylene glycol. The efficiency of crushing of the water granulated blast furnace slag and the fineness of powder of the slag can surely be increased.</p>
申请公布号 JPH0459061(A) 申请公布日期 1992.02.25
申请号 JP19900162684 申请日期 1990.06.22
申请人 UBE IND LTD 发明人 HOTTA TOSHIHIKO;ITO KAZUO;MURAKAMI TAKANOBU
分类号 B02C23/06;C04B18/14 主分类号 B02C23/06
代理机构 代理人
主权项
地址