发明名称 MANUFACTURE OF FE-NI ALLOY
摘要 PURPOSE:To manufacture an Fe-Ni alloy having superior formability by adding a specified amt. of B to an Fe-Ni alloy having a specified compsn. and by carrying out final cold rolling at a specified draft and annealing at a specified temp. CONSTITUTION:0.003-0.03wt.% B is added to an Fe-Ni alloy consisting of 30-85wt.% Ni and the balance Fe with inevitable impurities. The B added alloy is cold rolled at >=60% draft in a final rolling stage and annealed at 900-1,200 deg.C. Thus, an alpha-brass type texture is obtd. with little change in the basic properties of the Fe-Ni alloy and an Fe-Ni alloy having much superior formability is manufactured.
申请公布号 JPS6452021(A) 申请公布日期 1989.02.28
申请号 JP19870207159 申请日期 1987.08.20
申请人 NIPPON YAKIN KOGYO CO LTD 发明人 OMORI TSUTOMU;TSUDA MASAOMI;EBATO KAZUO
分类号 C21D8/00;C21D8/04;C21D8/12;C22C19/03;C22C38/08;C22F1/10 主分类号 C21D8/00
代理机构 代理人
主权项
地址