发明名称 ARYLENE SULFIDE POLYMER HEAT TREATMENT
摘要 A method for stabilizing the Tmc of PPS subjected to heat treatment in a temperature range between 240 DEG C. and 320 DEG C., particularly during the heating process of an extrusion operation, by increasing the tmperature of the polymer through the 240 DEG C.-320 DEG C. range at a rate of at least 20 DEG C. per minute or by subsequently raising the temperature of the polymer to at least 350 DEG C. for a time sufficient to stabilize the Tmc of the polymer.
申请公布号 AU2888684(A) 申请公布日期 1984.12.20
申请号 AU19840028886 申请日期 1984.05.31
申请人 PHILLIPS PETROLEUM CO. 发明人 ROY FRANKLIN WRIGHT
分类号 C08G75/02;C08G75/06 主分类号 C08G75/02