发明名称 |
HIGH RATE CARBON CATHODE, METHOD OF MAKING, AND ELECTROCHEMICAL CELL INCLUDING THE CATHODE |
摘要 |
A high rate carbon cathode is made by mixing a carbon powder having a surface area of about 1000 square meters/gram with polytetrafluoroethylene and a sufficient amount of water to form a coherent mixture. The mixture is applied to an electrically conductive screen; the cathode formed while wet to an intermediate thickness, the cathode vacuum dried at about 100 degrees C. and the cathode cold compressed to obtain a final electrode porosity of greater than 80 percent. The cathode can be used in lithium primary cell using a solution of an inorganic lithium salt in sulfuryl chloride as the electrolyte. |
申请公布号 |
CA1149449(A) |
申请公布日期 |
1983.07.05 |
申请号 |
CA19800365694 |
申请日期 |
1980.11.18 |
申请人 |
UNITED STATES (GOVERNMENT OF THE), AS REPRESENTED BY THE SECRETAR |
发明人 |
GILMAN, SOL |
分类号 |
H01M4/96 |
主分类号 |
H01M4/96 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|