发明名称 REGENERATION OF ZEOLITE CATALYST
摘要 A method is provided for regeneration of a catalyst comprising a crystalline aluminosilicate zeolite characterized by a silica to alumina mole ratio of at least about 12, a constraint index, as hereinafter defined, within the approximate range of 1 to 12, which catalyst has undergone controlled precoking by exposing the same to a thermally decomposable organic compound at a temperature in excess of the decomposition temperature of said compound but less than about 1200 DEG F., at a hydrogen to organic compound mole ratio of between 0 and 1 to deposit at least about 1 weight percent coke thereon, such precoked catalyst having been deactivated by formation of a carbonaceous deposit thereon as a result of use of the same in catalytically converting an organic charge under conditions less severe, i.e., at a lower temperature and/or a higher hydrogen concentration than those employed during said precoking which comprises contacting the aged catalyst with an atmosphere comprising hydrogen at a temperature between about 800 DEG F. and about 1200 DEG F. and a pressure between about 0 and about 2000 psig for a period of time sufficient to at least partially restore the activity of the catalyst.
申请公布号 ZA7904816(B) 申请公布日期 1981.04.29
申请号 ZA19790004816 申请日期 1979.09.11
申请人 MOBIL OIL CORP 发明人 RODEWALD P;KAETING W;HAAG W;OLSON D
分类号 B01J29/90;B01J38/10;C07B61/00;C07C1/00;C07C1/20;C07C2/66;C07C5/27;C07C6/12;C07C15/02;C07C15/08;C07C67/00 主分类号 B01J29/90
代理机构 代理人
主权项
地址