发明名称 REINFORCING METHOD OF CEMENT BUILDING MATERIAL
摘要 A building material such as cement brick was reinforced by dipping in the mixed soln. of synthetic resin soln. 70-80%, aluminium sulfate or alunite soln. 20-30% at a reducing pressure for 2 hr and drying at 100≦̸C for 15 min to give the water-resistant and high strength product with undenatured coating layer.
申请公布号 KR800001425(B1) 申请公布日期 1980.12.05
申请号 KR19780002892 申请日期 1978.09.21
申请人 PARK NO YANG;SHIN HYUNG KYUN 发明人 PARK NO YANG;SHIN HYUNG KYUN
分类号 (IPC1-7):C04B41/22 主分类号 (IPC1-7):C04B41/22