High yield semichemical wood pulping process |
摘要 |
70 To 85% yield semichemical wood pulping may be prepared for mechanical defibration by cooking comminuted hardwood in a continuous digestion vessel with an alkaline cooking solution wherein 50 to 100% as sodium oxide thereof is sodium carbonate. The solution may be formulated from unmodified kraft recovery process green liquor or, if a sulfur free cooking process is desired, the solution may be formulated from soda ash.
|