发明名称 時効硬化型ベイナイト非調質鋼
摘要 Hardened microalloyed bainitic steel comprises 0.06-0.18 wt.% of carbon (C), 0.01-0.60 wt.% of silicon (Si), 0.10-3 wt.% of manganese (Mn), 0.001-0.030 wt.% of sulfur (S), 0.001 -0.40 wt.% of copper (Cu), 0.001-0.40 wt.% of nickel (Ni), 0.10-2 wt.% of chromium (Cr), 0.01-1 wt.% of molybdenum (Mo), 0.20-0.45 wt.% of vanadium (V) and balance of iron (Fe) and incidental impurities. Hardened microalloyed bainitic steel comprises 0.06-0.18 wt.% of carbon (C), 0.01-0.60 wt.% of silicon (Si), 0.10-3 wt.% of manganese (Mn), 0.001-0.030 wt.% of sulfur (S), 0.001 -0.40 wt.% of copper (Cu), 0.001-0.40 wt.% of nickel (Ni), 0.10-2 wt.% of chromium (Cr), 0.01-1 wt.% of molybdenum (Mo), 0.20-0.45 wt.% of vanadium (V) and balance of iron (Fe) and incidental impurities. A value of expression of 15x [C]-[Mo]-2x V (1) is = 1.4. A value of expression of 4x [C]+[Si]+4x [Mn]+[Cu]+[Ni]+5x [Cr]+4x [Mo]+5x [V] (2) is = 16.5. A value of expression of 3x [C]+10x [Mn]+2x [Cu]+2x [Ni]+12x [Cr]+9x [Mo]+2x [V] (3) is 20-35.
申请公布号 JP5974623(B2) 申请公布日期 2016.08.23
申请号 JP20120111883 申请日期 2012.05.15
申请人 大同特殊鋼株式会社 发明人 大橋 亮介;木村 和良
分类号 C22C38/00;C22C38/58 主分类号 C22C38/00
代理机构 代理人
主权项
地址