发明名称 |
EARLY STRENGTH DEVELOPMENT TYPE, HIGH-FLUIDITY, LOW-HEAT, HIGH-DURABILITY, AND CARBON DIOXIDE REDUCTION TYPE CONCRETE COMPOSITION |
摘要 |
An early strength development type, high-fluidity, low-heat, high-durability, and carbon dioxide reduction type concrete composition of the present invention comprises: 10 to 40 parts by weight of fly ash; 10 to 40 parts by weight of Portland cement; 10 to 40 parts by weight of calcium carbonate; 5 to 20 parts by weight of crushed stone powder; 1 to 10 parts by weight of an activator; and 1 to 3 parts by weigh of a superplasticizer, on the basis of 100 parts by weight of ground granulated blast furnace slag (GGBFS). |
申请公布号 |
WO2015199291(A1) |
申请公布日期 |
2015.12.30 |
申请号 |
WO2014KR10691 |
申请日期 |
2014.11.07 |
申请人 |
DAEWOO ENGINEERING & CONSTRUCTION CO., LTD |
发明人 |
KIM, YONG JIC;KIM, YOUNG JIN;KIM, IN GYU;JO, JUN HEE;AN, TAE HO;JEON, YOUNG SU |
分类号 |
C04B18/08;C04B14/28;C04B18/14;C04B28/04 |
主分类号 |
C04B18/08 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|