摘要 |
The invention is directed to a process for the manufacture of heterophasic propylene copolymer compositions comprising the steps of forming a propylene polymer matrix in at least one slurry reactor and optionally in at least one gas phase reactor and subsequently forming in at least one gas phase reactor an elastomeric copolymer by copolymerizing propylene with ethylene and/or with another α-olefin in the presence of said matrix, wherein the polymerization is carried out in the presence of a catalyst system comprising a catalyst in form of solid particles, said particles: (a) have a surface area of less than 20 m/g, (b) comprise a transition metal compound of groups 4 to 10 of the periodic table or a compound of actinide or lanthanide, (c) comprise a metal compound of groups 1 to 3 of the periodic table, and (d) comprise inclusions not comprising catalytically active sites. |