发明名称 COMPOSITE FORMATION MATERIAL, SURFACE TREATED GLASS SHORT FIBER AND METHOD FOR MANUFACTURING COMPOSITE FORMATION MATERIAL
摘要 <p>A composite molding material formed by kneading at least glass wool into a thermoplastic resin has such a feature that the glass wool in the composite molding material has a fiber diameter of 1 to 7μm, an average fiber length of 30 to 300μm, and an aspect ratio of not less than 10.</p>
申请公布号 KR101456750(B1) 申请公布日期 2014.10.31
申请号 KR20120112482 申请日期 2012.10.10
申请人 发明人
分类号 C08J5/08;C08K7/14;C08K9/06;C08L101/00 主分类号 C08J5/08