发明名称 METHOD FOR PREPARING NONSHRINKAGE AE CONCRETE AND NONSHRINKAGE AE CONCRETE
摘要 <P>PROBLEM TO BE SOLVED: To provide a method for preparing nonshrinkage AE concrete with which the shrinkage factor of an obtained hardened product is suppressed to 50 &mu;m or less and the hardened product can be made into nonshrinkage substantially without adversely affecting the fluidity or the amount of entrained air of the prepared AE concrete, and the compression strength or neutralization suppression of the obtained hardened product. <P>SOLUTION: In the preparation of AE concrete using cement, fine aggregate, coarse aggregate, a dry shrinkage reducing agent, an expander, a cement dispersant, an air amount adjusting agent and water, high-early-strength portland cement is used as cement in a specific ratio, and specific blast furnace slag fine aggregate is used at least as a part of fine aggregate in a specific ratio. Concurrently, the dry shrinkage reducing agent and the expander are used in a specific ratio and the unit amount ratio is controlled into a specific range. <P>COPYRIGHT: (C)2013,JPO&INPIT
申请公布号 JP2012211040(A) 申请公布日期 2012.11.01
申请号 JP20110077288 申请日期 2011.03.31
申请人 TAKENAKA KOMUTEN CO LTD;TAKEMOTO OIL & FAT CO LTD 发明人 INOUE KAZUMASA;MITSUI TATEO;MISAWA DAISUKE;KINOSHITA MITSUO;SAITO KAZUHIDE;INAGAKI JUNJI;KOBAYASHI RYUHEI
分类号 C04B28/04;C04B14/06;C04B18/14;C04B22/06;C04B24/02;C04B24/26;C04B24/32;C08F220/06 主分类号 C04B28/04
代理机构 代理人
主权项
地址