发明名称 AU + CU BASE-AG-ZN ALLOY
摘要 A gold alloy classified into 8 to 12 carats contains 30.0 to 50.0% by weight of gold and the remainder is an alloying composition which includes 75.2-77.1% of copper, 13.6 to 16.2% of silver and 6.7 to 11.2% of zinc. The preferred alloys are 9 and 10 carats. The alloys exhibit satisfactory color tone and luster and have improved physical and chemical properties including workability, hardness, chemical resistance and perspiration resistance. The alloys are fabricated into articles which are surface finished by buffing or electrolytic polishing.
申请公布号 AU523626(B2) 申请公布日期 1982.08.05
申请号 AU19800054315 申请日期 1980.01.03
申请人 MURAO SHOTEN K.K. 发明人 MASAMI MURAO
分类号 C22C30/00;C22C5/02;C22C9/00;C22C30/02;C22C30/04;C22C30/06 主分类号 C22C30/00
代理机构 代理人
主权项
地址