摘要 |
PROBLEM TO BE SOLVED: To provide a method of manufacturing particulate dispersion body, capable of very easily giving conductivity, dispersibility, dispersion stability, transparency, precipitation preventing properties, and the like to the particulate dispersion body, or improving them, and the particulate dispersion body manufactured by this method. SOLUTION: First, one or more kinds selected from among a group constitutted of organic metal compounds and organic semimetal compounds are mixed with a reducing agent and to prepare a mixture 12. Subsequently, the mixture 12 is heated to a temperature of 40-360°C, in a prescribed atmosphere and kept in that state for 10 minutes to 5 hours to obtain the dispersion 14 in which the particulates are dispersed. The heated atmosphere of the mixture 12 is, preferably an inert-gas atmosphere, a reducing-gas atmosphere, or an air atmosphere. COPYRIGHT: (C)2011,JPO&INPIT |