发明名称 DECOMPOSITION METHOD OF CELLULOSE AND PRODUCTION METHOD OF GLUCOSE
摘要 A method for decomposing cellulose to be contained in a cellulose raw material is provided. A pulverized cellulose based biomass is enclosed in a pressure closed vessel, and a sodium hydroxide aqueous solution having a concentration of %, pure water and 5 g of nickel oxyhydroxide obtained by solid-solving therein at least one kind of zinc, aluminum, magnesium, calcium, manganese, cobalt, copper and tin relative to nickel are added to prepare a catalytic reaction solution. Next, the catalytic reaction solution for decomposing cellulose by using nickel oxyhydroxide as a catalyst is subjected to a decomposition reaction of cellulose while stirring by using a stirring blade and heating at a temperature rising rate of 5.degree.C/min. The reaction is carried out under autogenous pressure (saturated vapor pressure of water) in the reactor. After the temperature of the catalytic reaction solution has reached a prescribed temperature, the resulting catalytic reaction solution is heated for one hour and then cooled to room temperature at a rate of about 3.degree.C/min.
申请公布号 CA2625383(A1) 申请公布日期 2008.09.16
申请号 CA20082625383 申请日期 2008.03.13
申请人 SEIKO INSTRUMENTS INC. 发明人 YAMAGUCHI, NORISHIGE
分类号 C13K1/02;B01J23/755;C07H3/00;C07H3/02 主分类号 C13K1/02
代理机构 代理人
主权项
地址