发明名称 PRODUCTION METHOD OF SLAG CRUSHED STONE
摘要 PROBLEM TO BE SOLVED: To provide the production method of slag crushed stone, by which the dust preventing measure in the transportation and the mixing is dispensed with, the blending of carbon-containing waste for preventing the solidification is unnecessary, and the crushed stone having small coefficient of expansion is obtained by uniformizing the water content during aging. SOLUTION: In the production of the slag crushed stone by adding coal ash to steel slag or molten iron pre-treatment slag and carrying out aging, coal ash in which water content is previously controlled to 10-30% is used. As a result, the dust preventing measure in the transportation and the mixing is dispensed with. Further the aging is accelerated by keeping the water content in the coal ash to 10-30% during the steam aging to obtain the slag crushed stone having small coefficient of expansion. COPYRIGHT: (C)2006,JPO&NCIPI
申请公布号 JP2006001776(A) 申请公布日期 2006.01.05
申请号 JP20040178479 申请日期 2004.06.16
申请人 NIPPON STEEL CORP;KYOZAI SAISEKI KK 发明人 WATANABE HIDEMI;TANAKA HISAO;HASHIYAMA KAZUO;KAMEYAMA EIJI
分类号 C04B5/06;B09B3/00;C21C1/02;C21C5/28;C21C5/54 主分类号 C04B5/06
代理机构 代理人
主权项
地址