发明名称 METHOD FOR FORMING OPTICAL FIBER
摘要 <p><P>PROBLEM TO BE SOLVED: To reduce attenuation of a glass optical fiber due to heat aging and Rayleigh scattering in a heat treatment of the fiber. <P>SOLUTION: In the method for forming an optical fiber, the optical fiber is formed by drawing at≥10 m/sec draw rate from a heated glass source (block 10) and is heat-treated by maintaining the optical fiber within a heated treatment zone for the total resident time of 0.07-0.25 sec, while subjecting the optical fiber to an average cooling rate of 1,200-5,000°C/sec defined by ä[fiber surface temperature in an inlet zone]-[fiber surface temperature in the outlet zone]}/[the total resident time of the optical fiber in the treatment zone] (block 20). <P>COPYRIGHT: (C)2005,JPO&NCIPI</p>
申请公布号 JP2005162610(A) 申请公布日期 2005.06.23
申请号 JP20050016570 申请日期 2005.01.25
申请人 CORNING INC 发明人 FOSTER JOHN D;DANIEL W HOOTOFU;LACY CLAUDE L;PENG YING LISA;POWERS DALE R;TARPLEE JENNIFER L;MATTHEWS HAZEL B;MIECZKOWSKI DANIEL;QUINN RICHARD A;WALCZAK WANDA J
分类号 C03B37/12;C03B37/027;G02B6/00;(IPC1-7):C03B37/027 主分类号 C03B37/12
代理机构 代理人
主权项
地址