摘要 |
PROBLEM TO BE SOLVED: To provide a method for producing a low interadhesive polyethylene pellet consecutively and efficiently. SOLUTION: The low interadhesive polyethylene pellet comprises a straight low density polyethylene having a density of 935 kg/m<SP>3</SP>or less, at least 0.5-25 wt% of talc, and 100-10,000 wt.ppm of a lubricant. In the preferable embodiment of the invention, the lubricant is erucic acid amide; the low interadhesive polyethylene has a density of 860-880 kg/m<SP>3</SP>; the talc has a content of 0.8-1.0 wt%; and the lubricant has a content of 500-5,000 wt.ppm, particularly preferably 1,000-2,000 wt.ppm. COPYRIGHT: (C)2005,JPO&NCIPI |