Process for making a high temperature-resistant ceramic material with an adjustable thermal expansion coefficient and method of use of same |
摘要 |
The process for making the high temperature-resistant ceramic material from the MgO-Al2O3 system includes burning a mixture containing a predetermined amount of magnesium oxide (MgO) of a predetermined grain size distribution in an amount range of from 30 to 99 parts by weight and a predetermined amount of magnesium aluminate (MgAl2O4) of another different predetermined grain size distribution in a range of from 1 to 70 parts by weight to obtain a ceramic product having a thermal expansion coefficient and selecting the amounts of magnesium oxide and magnesium aluminate as well as the predetermined grain size distributions so that the thermal expansion coefficient of the ceramic product is substantially equal to that of platinum and platinum alloys and in a range of from 9x10-6 K-1 to 15x10-6 K-1.
|
申请公布号 |
US6274525(B1) |
申请公布日期 |
2001.08.14 |
申请号 |
US19990359273 |
申请日期 |
1999.07.22 |
申请人 |
SCHOTT GLAS |
发明人 |
ZBOROWSKI JANUSZ;EICHHORN UWE;ALOY-DOLS BARTOLOME |
分类号 |
C03B5/167;C03B5/43;C03B37/095;C04B35/043;C04B35/053;C04B35/443;C04B35/66;C04B41/51;C04B41/88;(IPC1-7):C04B35/03 |
主分类号 |
C03B5/167 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|